The effects of degassing, grain refinement & Sr-addition on melt quality-hot tear sensitivity relationships in cast A380 aluminum alloy

dc.authorid0000-0001-9150-3292en_US
dc.contributor.authorUludağ, Muhammet
dc.contributor.authorCetin, Remzi
dc.contributor.authorDispinar, Derya
dc.contributor.authorTiryakioglu, Murat
dc.date.accessioned2021-03-20T20:13:07Z
dc.date.available2021-03-20T20:13:07Z
dc.date.issued2018
dc.departmentBTÜ, Mühendislik ve Doğa Bilimleri Fakültesi, Metalurji ve Malzeme Mühendisliği Bölümüen_US
dc.description.abstractHot tearing tendency of A380 with various element additions (Sr, Sr + Ti, Ti, B and B + Sr) was investigated. Constrained rod casting (CRC) hot tearing test method was used to characterize the hot tearing sensitivity. Reduced pressure test (RPT) samples were produced from each condition and all trials were repeated three times. Number density of pores on the cross section of RPT samples was calculated via digital image processing and statistical analysis was carried out. Microstructure analysis was carried out to observe the effect of alloying elements. Hot torn cross sections were subjected to SEM analysis. It was found that in aluminum alloys, the most deleterious defects, bifilms that are the cause of many defects, play an important role in initiating the hot tearing during solidification. It is important to note that the shape, size and distribution of bifilms are too complex. They act as heterogeneous nucleation site for liquid to separate and thus increase hot tearing.en_US
dc.description.sponsorshipScientific Research Projects Coordination Unit of Selcuk UniversitySelcuk University [13101026]; TUBITAK (Turkey)Turkiye Bilimsel ve Teknolojik Arastirma Kurumu (TUBITAK) [1059B141401190]en_US
dc.description.sponsorshipThis work has been supported by the Scientific Research Projects Coordination Unit of Selcuk University (Project number: 13101026). Author would like to thanks to TUBITAK (1059B141401190) (Turkey) for its supporting.en_US
dc.identifier.doi10.1016/j.engfailanal.2018.03.025en_US
dc.identifier.endpage102en_US
dc.identifier.issn1350-6307
dc.identifier.issn1873-1961
dc.identifier.scopusqualityQ1en_US
dc.identifier.startpage90en_US
dc.identifier.urihttp://doi.org/10.1016/j.engfailanal.2018.03.025
dc.identifier.urihttps://hdl.handle.net/20.500.12885/794
dc.identifier.volume90en_US
dc.identifier.wosWOS:000432858400008en_US
dc.identifier.wosqualityQ2en_US
dc.indekslendigikaynakWeb of Scienceen_US
dc.indekslendigikaynakScopusen_US
dc.institutionauthorUludağ, Muhammet
dc.language.isoenen_US
dc.publisherPergamon-Elsevier Science Ltden_US
dc.relation.ispartofEngineering Failure Analysisen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectDegassingen_US
dc.subjectGrain refinementen_US
dc.subjectModificationen_US
dc.subjectBifilmsen_US
dc.subjectHot tearingen_US
dc.titleThe effects of degassing, grain refinement & Sr-addition on melt quality-hot tear sensitivity relationships in cast A380 aluminum alloyen_US