Effect of Water and Air Curing Conditions on the Compressive Strength of Concrete Incorporating Mineral and Chemical Admixtures

dc.authorid0000-0001-6685-2319
dc.authorid0000-0001-5522-427X
dc.authorid0000-0001-7085-4819
dc.authorid0000-0003-0326-5015
dc.contributor.authorBenlioğlu, Arif
dc.contributor.authorÖzen, Süleyman
dc.contributor.authorYıldırım, Musa
dc.contributor.authorMardani, Ali
dc.date.accessioned2026-11-20T06:34:10Z
dc.date.issued2026
dc.departmentBTÜ, Mühendislik ve Doğa Bilimleri Fakültesi, İnşaat Mühendisliği Bölümü
dc.description.abstractCuring conditions play a critical role in the strength development of concrete. In particular, determining the influence of different curing regimes on the mechanical performance of concrete incorporating both mineral and chemical admixtures is essential for the development of sustainable concrete technologies. In this study, the compressive strength of concrete produced by separately replacing 10% of the cement with either blast furnace slag or fly ash was investigated. For each binder system, three concrete mixtures were prepared: a control mixture containing a superplasticizer but no set accelerator or set retarder, a mixture containing a set accelerator, and a mixture incorporating a set retarder. Specimens were tested at curing ages of 7, 28, and 56 days under two different curing regimes. In the first regime, the specimens were continuously cured in water throughout the entire curing period, whereas in the second regime, they were stored under laboratory air conditions for the same duration. Accordingly, the effects of water curing and air curing on the compressive strength development of concrete containing different binder systems and chemical admixtures were comparatively evaluated. The results demonstrated that the compressive strength was governed by the combined effects of curing age, curing regime, mineral admixture type, and chemical admixture type. For all mixtures, specimens subjected to water curing exhibited higher compressive strengths than those exposed to air curing, with the difference becoming more pronounced at 28 and 56 days. Although water curing consistently resulted in higher absolute compressive strengths, the relative effects of the accelerating and retarding admixtures varied depending on curing condition, binder composition, and testing age. Although concrete incorporating 10% blast furnace slag and fly ash exhibited lower compressive strength than the control concrete at early ages, it exceeded the strength of the control concrete after 56 days of water curing. Furthermore, the set accelerator enhanced early-age strength development, whereas the set retarder promoted greater long-term strength development, particularly under water curing conditions.
dc.identifier.citationBenlioğlu, A., Özen, S., Yıldırım, M., & Mardani, A. (2026, October 30). Effect of Water and Air Curing Conditions on the Compressive Strength of Concrete Incorporating Mineral and Chemical Admixtures. 7. International Paris Congress on Applied Sciences, Paris, France.
dc.identifier.endpage559
dc.identifier.isbn979-8-89695-599-3
dc.identifier.startpage548
dc.identifier.urihttps://hdl.handle.net/20.500.12885/7121
dc.institutionauthorBenlioğlu, Arif
dc.institutionauthorÖzen, Süleyman
dc.institutionauthorYıldırım , Musa
dc.institutionauthorid0000-0001-6685-2319
dc.institutionauthorid0000-0001-5522-427X
dc.institutionauthorid0000-0001-7085-4819
dc.language.isoen
dc.publisherLiberty Academic Publishers
dc.relation.ispartof7. International Paris Congress on Applied Sciences 28-30 September
dc.relation.publicationcategoryKonferans Öğesi - Uluslararası - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectAir Curing
dc.subjectChemical Admixtures
dc.subjectCompressive Strength
dc.subjectFly Ash
dc.subjectBlast Furnace Slag
dc.subjectWater Curing
dc.titleEffect of Water and Air Curing Conditions on the Compressive Strength of Concrete Incorporating Mineral and Chemical Admixtures
dc.typeConference Object

Dosyalar

Orijinal paket

Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
EFFECT OF WATER AND AIR CURING CONDITIONS ON THE COMPRESSIVE STRENGTH OF CONCRETE INCORPORATING MINERAL AND CHEMICAL ADMIXTURES.pdf
Boyut:
1,44 MB
Biçim:
Adobe Portable Document Format