Effect of Alkali Activator Type and Hydroxide-to-Silicate Ratio on the Fresh and Mechanical Properties of Ground Granulated Blast Furnace Slag-Based Geopolymer Pastes

dc.authorid0000-0001-6685-2319
dc.authorid0000-0002-5176-9990
dc.authorid0000-0001-5522-427X
dc.authorid0000-0003-0326-5015
dc.contributor.authorBenlioğlu, Arif
dc.contributor.authorYüksel, İsa
dc.contributor.authorÖzen, Süleyman
dc.contributor.authorMardani, Ali
dc.date.accessioned2026-11-20T06:34:17Z
dc.date.issued2026
dc.departmentBTÜ, Mühendislik ve Doğa Bilimleri Fakültesi, İnşaat Mühendisliği Bölümü
dc.description.abstractThis study investigated the effects of different alkali activator combinations and hydroxide-to-silicate (H/S) ratios on the fresh and hardened properties of ground granulated blast furnace slag (GGBFS)-based geopolymer pastes. Four alkali activator systems, namely sodium silicate–sodium hydroxide (NaS–NaH), sodium silicate–potassium hydroxide (NaS–KH), potassium silicate–sodium hydroxide (KS–NaH), and potassium silicate–potassium hydroxide (KS–KH), were prepared using sodium silicate (Na₂SiO₃), potassium silicate (K₂SiO₃), sodium hydroxide (NaOH), and potassium hydroxide (KOH) solutions. The activator-to-binder ratio was maintained constant at 0.50 for all mixtures, while the hydroxide-to-silicate (H/S) ratio was varied at 0.55, 0.65, 0.75, and 0.85. The prepared geopolymer paste specimens were cured at room temperature (25 ± 2 °C) for 28 days. The fresh properties of the geopolymer pastes were evaluated through the flow spread test, whereas the hardened properties were assessed by compressive strength, flexural strength, and water absorption tests. The experimental results demonstrated that both the H/S ratio and the alkali activator composition had a significant influence on the fresh and hardened properties of the geopolymer pastes. Increasing the H/S ratio from 0.55 to 0.85 improved the workability of all mixtures but generally resulted in reductions in compressive and flexural strengths and an increase in water absorption. Among the investigated activator systems, the sodium silicate–potassium hydroxide (NaS–KH) combination more effectively promoted the geopolymerization reaction, resulting in superior mechanical performance compared with the other activator systems. The highest compressive and flexural strengths were obtained for the NaS–KH mixture with an H/S ratio of 0.55, reaching 118.98 MPa and 5.87 MPa, respectively. The findings indicate that the combined optimization of alkali activator composition and the hydroxide-to-silicate ratio plays a critical role in achieving a balanced combination of workability, mechanical performance, and durability-related properties in GGBFS-based geopolymer pastes.
dc.identifier.citationBenlioğlu, A., Yüksel, I., Özen, S., & Mardani, A. (2026, October 30). Effect of Alkali Activator Type and Hydroxide-to-Silicate Ratio on the Fresh and Mechanical Properties of Ground Granulated Blast Furnace Slag-Based Geopolymer Pastes. 7. International Paris Congress on Applied Sciences, Paris, France.
dc.identifier.endpage587
dc.identifier.isbn979-8-89695-599-3
dc.identifier.startpage577
dc.identifier.urihttps://hdl.handle.net/20.500.12885/7123
dc.institutionauthorBenlioğlu, Arif
dc.institutionauthorYüksel , İsa
dc.institutionauthorÖzen, Süleyman
dc.institutionauthorid0000-0001-6685-2319
dc.institutionauthorid0000-0002-5176-9990
dc.institutionauthorid0000-0001-5522-427X
dc.language.isoen
dc.publisherLiberty Academic Publishers
dc.relation.ispartof7. International Paris Congress on Applied Sciences 28-30 September
dc.relation.publicationcategoryKonferans Öğesi - Uluslararası - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectGeopolymer Paste
dc.subjectHydroxide-to-Silicate Ratio
dc.subjectMechanical Properties
dc.subjectPotassium
dc.subjectSodium
dc.titleEffect of Alkali Activator Type and Hydroxide-to-Silicate Ratio on the Fresh and Mechanical Properties of Ground Granulated Blast Furnace Slag-Based Geopolymer Pastes
dc.typeConference Object

Dosyalar

Orijinal paket

Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
EFFECT OF ALKALI ACTIVATOR TYPE AND HYDROXIDE-TO-SILICATE RATIO ON THE FRESH AND MECHANICAL PROPERTIES OF GROUND GRANULATED BLAST FURNACE SLAG-BASED GEOPOLYMER PASTES.pdf
Boyut:
1,2 MB
Biçim:
Adobe Portable Document Format